Table 5.

Obtained results and calculated amounts of PEI molecules from thermogravimetric analysis for surface-modified samples in different units.

Sample Weight Loss a
wt.%
Mass of Organic Part b
mg·g−1
Amount of Organic Part c
mmol·g−1
SBA-15(C)-Cl 6.01 58.8 -
SBA-15(C)-800 9.80 92.6 0.116
SBA-15(C)-1300 14.95 146.5 0.113
SBA-15(C)-2000 24.02 237.5 0.118

a—mass losses in wt.% on TG curves in the temperature range of 150–800 °C; b—the mass of PEI molecules in mg on the surface of support per 1 g of material; c—the amount of PEI molecules in mmol on the surface of support per 1 g of material.