Skip to main content
. 2021 Apr 11;13(8):1233. doi: 10.3390/polym13081233

Figure 3.

Figure 3

XRD pattern for (a) pure CS, (b) CSDN2, and (c) CSDN3 electrolytes over the range of 5–80° with a step size of 0.1°.