Skip to main content
. 2021 Apr 12;13(8):1247. doi: 10.3390/polym13081247

Table 4.

TGA thermal parameters and degree of crystallinity determined by DSC for all films at different disintegration times.

Film Sample Disintegration Time (Days) T5% (°C) Tmax (°C) Residue at 800 °C (%) Xc (%)
PLA-V 0 325 366 1.5 2
4 270 319 1.3 35
11 245 339 1.3 -
PLA-f 0 323 359 1.5 1
4 288 338 0.8 24
11 257 348 1.1 -
3D-PLA 0 323 359 1.5 2
4 285 332 2.2 24
11 249 340 0.6 -
3D-PLA-R 0 321 359 1.5 1
4 285 331 1.3 25
11 248 344 0.6 -
Cor-PLA-R 0 303 357 1.5 4
4 260 332 1.7 37
11 250 343 1.4 -