Skip to main content
. 2021 Apr 9;13(8):1218. doi: 10.3390/polym13081218

Table 2.

Plate-plate rheometry (PPR)-based modified cross-law parameters for HDPE melt at 200 °C.

Parameter Unit Material 1 Material 2 Material 3
η0 Pa.s 43,226 4559 1930
λ s 0.362 0.125 0.0711
m - 0.761 0.571 0.491