Dielectric loss factor tan δ of the POx-based materials at 40 Hz.

SOE (wt.%) tan δ
No Filler BN
40 wt.%
n-AlN/μ-AlN
20/20 wt.%
BN/n-AlN/μ-AlN
20/10/10 wt.%
0 0.10 0.09 0.11 0.16
15 0.16 0.18 0.25 0.46
30 0.17 0.44 0.18 0.26