Figure 12.

Figure 12

Cross-section SEM of (a) epoxy coating (b) epoxy-CaCO3 coating, (c) epoxy-3 wt%SLS/CaCO3 coating, and (d) epoxy-5 wt%SLS/CaCO3 coating after exposure to the SCP solutions for 48 h.