a XRD patterns of the Ti3AlC2 before and after HF treatment at room temperature. b SEM image of a multilayer Ti3C2Tx after HF treatment. c Transmitted light micrographs of exfoliated Ti3C2Tx. d TEM images for Ti3C2Tx layers. e Thickness dependence of the reflection loss of the 50 wt% Ti3C2Tx filled Ti3C2Tx/wax composites in the Ku-band. Reproduced with permission from Ref. [119]. Copyright 2016, Elsevier. f High-resolution (HR) TEM image of D-Ti3C2Tx. g The selected area electron diffraction (SAED) pattern of D-Ti3C2Tx. h–k Reflection loss of composite with different D-Ti3C2Tx/wax weight fraction at different layer thickness.