Skip to main content
. 2021 Apr 21;13(9):1361. doi: 10.3390/polym13091361

Figure 10.

Figure 10

Fracture surfaces after tensile tests of PLA (a), OFI10 (b), OFI20 (c), POL10 (d) and POL20 (e) 3D-printed samples; scale bar 100 μm.