Skip to main content
. 2021 Apr 22;13(9):1369. doi: 10.3390/polym13091369

Table 4.

Tensile strength of untreated, alkali (NaOH)-treated, and single pineapple leaf fibres (PALF) epoxy composite [99].

PALF Young’s Modulus
(MPa)
Tensile Strength
(MPa)
Strain to Failure
(%)
Untreated 12.58 532.74 4.83
Alkali treated 15.72 635.44 4.38
Epoxy-coated PALF 14.33 534.88 3.86