Skip to main content
. 2021 Apr 23;14(9):2175. doi: 10.3390/ma14092175

Figure 1.

Figure 1

(a) Preparation of the bio-brick sample in a rigid mold in full contact. (b) Sketch drawing of batch reactor for immersion treatment method. Reprinted with permission from [58]. Copyright 2021 Elsevier.