Figure 5.

Figure 5

High-resolution TEM image (a) of the microstructure of the HPT-deformed Ti–3wt.% Nb alloy, pre-annealed at 600 °C with Fast Fourier Transforms (FFT) obtained from the marked squares for the α-phase (b) and ω-phase (c).