Enlarged part of the DSC heating curves of the deformed Ti–3wt.% Nb alloy pre-annealed at 450 and 600 °C (a). The XRD in situ heating map of the deformed Ti–3wt.% Nb alloy, pre-annealed at 600 °C (b). At the given 2θ angle interval, the ω-phase is presented by (11.0 + 10.1) a doublet of peaks.