Figure 8.

Figure 8

(a) Electrochemical charge and discharge curve of 30% Li1.25Cr0.25Mn1.5O4 and 70% LiNi0.5Mn1.5O4 solid solution formed at 850 °C (nominal composition: Li1.025Cr0.025Ni0.45Mn1.5O4) (b) Discharge capacity of Li1.075Cr0.075Ni0.35Mn1.5O4 as function of charge and discharge rate at a loading of about 6 mg cm−1 (~ 0.7 mAh cm−1). Symmetrical charge and discharge rate indicated on the figure were varied each five cycles (cycles 1–30) and fixed at 1C for cycles 31–60.