Skip to main content
. 2021 May 20;8:15. doi: 10.1186/s40580-021-00265-8

Table 2.

Roughness of electrically conductive films containing untreated Ag/Cu and alkanethiol-modified Ag/Cu powders

Sample Ra (µm) Rz (µm)
Ag/Cu 2.043 ± 0.15 13.459 ± 1.54
Ag/Cu-C4 0.719 ± 0.17 8.408 ± 1.13
Ag/Cu-C8 0.760 ± 0.13 8.608 ± 1.01