Skip to main content
. 2021 May 13;7(5):e07008. doi: 10.1016/j.heliyon.2021.e07008

Figure 6.

Figure 6

Comparison of samples with polyethylene as sole carbon source for the control sample and biodegraded sample after a period of 40 days.