Skip to main content
. 2021 Apr 23;13(5):614. doi: 10.3390/pharmaceutics13050614

Table 1.

Summary of XPS atomic concentration, contact angle, and surface roughness from AFM for various treated Nylon tubes.

Sample XPS Atomic Concentration (%) Contact Angle (°) RMS Roughness (nm)
C1s O1s N1s P2p
Nylon 85.09 10.47 4.43 - 92.46 28.483
PVP 81.95 10.71 7.35 - 60.2 79.304
PVP/Lipo+EVL 84.7 12.09 1.71 1.5 19.26 135.18
PVP/Lipo+EVL/PVP 81.95 10.51 7.54 - 33.83 162.80

PVP: polyvinylpyrrolidone; Lipo + EVL: Everolimus-loaded liposome; XPS: X-ray photoelectron spectroscopy; RMS: Root mean square.