Skip to main content
. 2021 May 13;13(10):1565. doi: 10.3390/polym13101565

Figure 10.

Figure 10

Morphology of EPDM foams produced under different temperatures: (a) 140 °C, (b) 150 °C and (c) 160 °C [199].