Skip to main content
. 2021 May 7;93(19):7180–7187. doi: 10.1021/acs.analchem.0c04944

Figure 3.

Figure 3

Variation in mass of tiles cast from 16 commercially available SLA resins, after 2 h of UV post-curing at 405 nm (blue), or a combined UV post-curing and 4 h post-baking at 120 °C (red), expressed as % of the initial mass (n = 3).