Table 1. Melting Temperatures of Cross-Linked Copolymers Formed by PCLDIMAs of Different Molecular Masses and 25 wt % BA with 1 wt % BPO.

  melting temperature (°C)
Mw (g/mol) 400 600 2000 4000 8000 15000
400       24.5 47.1  
600       32.9 47.6  
2000           45.4
4000 24.5 32.9     45.5 53.5
8000 47.1 47.6   45.5    
15000     43.2 (1:1) 53.3    