Figure 2.

Figure 2

Drug-empty CDNs self-assemble into nanoparticles. (A) Table displaying the mean size, PDI, and ζ-potential for drug-empty nanoparticles formed by CDNs 14. (B) SEM image of representative Amine-CDN-3. (C) SEM image of representative CDN-4, which bears mPEG550 surface functionality. Scale bars = 1 μm. Errors are reported as standard deviations of at least three independently formulated batches.