. 2021 May 17;13(10):1610. doi: 10.3390/polym13101610

Figure 6.

Figure 6

Differential scanning calorimetry (DSC) curves (exo up), the second heating run, for neat PLA, PLA with MB/PEG bio-plasticizers: (a), and PLA-based biocomposites containing CS-M: (b).