Skip to main content
. 2021 May 14;13(10):1578. doi: 10.3390/polym13101578

Figure 4.

Figure 4

(A) Porosity and (B) swelling ratio of silk web prepared at various reeling velocities. Reeling bath temperature was 50 °C.