Skip to main content
. 2021 May 14;13(10):1578. doi: 10.3390/polym13101578

Table 3.

Photographs of 20 mm (width) × 50 mm (height) silk web (untreated) and silk non-woven fabrics (hot-pressed silk web) prepared at various reeling bath temperatures. Reeling velocity was 39.2 m/min.

Reeling Bath Temp. (°C) 25 50 70 90
Sample
Silk web graphic file with name polymers-13-01578-i008.jpg graphic file with name polymers-13-01578-i009.jpg graphic file with name polymers-13-01578-i010.jpg graphic file with name polymers-13-01578-i011.jpg
Silk non-woven fabric graphic file with name polymers-13-01578-i012.jpg graphic file with name polymers-13-01578-i013.jpg graphic file with name polymers-13-01578-i014.jpg graphic file with name polymers-13-01578-i015.jpg