. 2021 May 14;13(10):1587. doi: 10.3390/polym13101587

Figure 10.

Figure 10

The tension–tension fatigue test results for acrylonitrile butadiene styrene (ABS) parts with different raster orientation: longitudinal (0°), default (+45°/−45°), diagonal (45°), and transverse (90°) [90].