Skip to main content
. 2021 Jun 2;8(6):202375. doi: 10.1098/rsos.202375

Table 2.

The formulation of autoxidative water-reducible alkyd coating.

materials brand weight (g)
pigment pastes (75%) made in laboratory 30.0
water-reducible alkyd resin (80%) made in laboratory 31.3
distilled water made in laboratory 38.4
BCS Jiangxi Pinghai Biotechnology Co., Ltd 2.0
TEA Shanghai Aladdin Bio-Chem Technology Co., Ltd. 2.5
drier OXY-Coat 1101 0.2
wetting agent TEGO-245 0.2
levelling agent BYK-381 0.2