. 2021 Jun 2;11:11627. doi: 10.1038/s41598-021-90878-0

Table 2.

g-factors, integrated area of EPR signal, and the accurate defect concentration of carbon-based starting materials and B4C samples synthesized via various conditions.

g-factor (isotropic) Integrated area Defect concentration (spins/g)
Active C 2.0031 1.23 × 102 2.15 × 1017
Graphite 2.0098 2.82 × 102 4.93 × 1017
S1@G3 2.0023 4.81 × 103 8.41 × 1018
S2@G6 2.0031 2.52 × 103 4.41 × 1018
S3@A3 2.0025 5.36 × 101 9.38 × 1016
S4@A6 2.0027 4 × 103 7 × 1018