Failure modes on cracked surfaces of tested groups/subgroups.

Groups/subgroups Group I (zirconia) Group II (veneering ceramic) Group III (zirconia/veneering ceramic)
Subgroup I (control-grinding) 8 adhesive failure
2 mix failure
9 cohesive failure
1 mix failure
4 cohesive failure
1 adhesive failure
5 mix failure
Subgroup II (sandblasting) 8 adhesive failure
2 mix failure
8 cohesive failure
2 mix failure
4 cohesive failure
6 mix failure
Subgroup III (long-pulse laser) 10 adhesive failure 7 cohesive failure
1 adhesive failure
2 mix failure
4 cohesive failure
6 mix failure
Subgroup IV (short-pulse laser) 10 adhesive failure 7 cohesive failure
1 adhesive failure
2 mix failure
2 cohesive failure
8 mix failure