a Fabrication procedure for the flexible quasi-solid-state micro-ZHCs. b CV curves of the micro-ZHCs at different scan rates. c GCD curves at different current densities. d Areal capacity and rate capability. e GCD curves at 1 mA cm−2 of a single cell, and two cells connected in series or parallel. The inset shows two cells connected in series and good flexibility of the device. f GCD curves at 1 mA cm−2 of the micro-ZHCs under different bending angles from 0° to 180°