a) Change of preferred orientation of LCO thin films deposited for 30 min (denoted as (a), thickness ≈0.31 µm), 60 min (denoted as (b), thickness ≈0.77 µm), and 120 min (denoted as (c), thickness ≈1.35 µm) and b) correlated diffusion coefficients as a function of the amount of Li intercalated into the LCO structure as determined by GITT. Reproduced with permission.[ 96 ] Copyright 2008, Elsevier.