Skip to main content
. 2021 May 21;6(22):13953–13961. doi: 10.1021/acsomega.0c05204

Table 5. Semichar Stability Test Experiment for Lignitea.

final temperature (°C) accumulated gas flow (L) tar and water production (g) semichar yield (g) particle size (mm) particle size mass distribution (g) distribution percentage (%) volatile (%)
        >6 10.87 88.3 26.4
450 1.3 5.431 12.282 3–6 1.217 9.89 25.0
        <3 0.223 1.81
        total 12.31 100
        >6 10.903 94.86 12.6
550 1.8 5.386 11.476 3–6 0.459 3.99
        <3 0.132 1.15
        total 11.494 100
        >6 9.016 87.37 8.16
650 3.2 5.662 10.159 3–6 1.084 10.5 7.43
        <3 0.219 2.12
        total 10.319 100
a

″—″ in the table means that the quality is lower than the standard inspection quality.