Figure 4.

Figure 4

Tendency of discoloration. Discoloration tended to increase from the initial value for 7 days after immersion for all materials. From the top, the samples are of Custom-block, PMMA-disk, and Conventional PMMA. (a) Initial value; (b) 7 days after immersion.