Defects of steel pipelines produced during prefabrication and their causes [4,5,7,8,9,26,27].

Defects Location The Reason for the Formation
shrinkage cavity near-surface the last solidified of molten metal shrinks
casting hot crack internal and external surfaces stress due to different solidification rate
stoma surface or near-surface the gas is retained when the metal solidifies
inclusion surface or near-surface impurities were added into the casting process
cracks surface the surface depression is discontinuous and elongated during rolling
layered surface or near-surface inherent defects are elongated and flattened during the rolling
fold surface excess material covering and pressing into surfaces
heat treatment crack surface uneven heating or cooling
coating crack surface residual stress release