Table 1.
Parameters | Unit of Measure |
Cabuya Fiber |
Zeolites |
---|---|---|---|
Clinoptilolite Mordenite Sodium Mordenite | |||
Effective porosity | 0.55 | 0.30 | |
Density | kg/m3 | 16 | 100 |
Mass of the reactive material | kg | 0.030 | 0.083 |
Column diameter | m | 0.042 | |
Column area | m2 | 0.0014 | |
Height of the reactive column | m | 0.18 | |
Reactive column volume | L | 25 | |
Metal concentration | mg/L | Zn: 100; Cu: 30; Cd: 4 | |
Flow rate | L/h | 0.0216 | |
Velocity | m/h | 0.016 |