Skip to main content
. 2021 Jun 21;12:3814. doi: 10.1038/s41467-021-24120-w

Table 1.

Compositions of cationic elements in pristine Li(Ni0.80Co0.15Mn0.05)O2 (NCM) and NCM subjected to 100 and 300 cycles as measured by ICP-AES (the atomic concentration is normalised to obtain a total TM fraction of 1).

Specimen Atomic concentration (weight %)
Li Ni Co Mn
NCM-pristine 1.04 (6.77) 0.80 (44.31) 0.15 (8.24) 0.05 (2.46)
NCM-100 cycles 0.94 (6.16) 0.80 (44.36) 0.15 (8.23) 0.05 (2.46)
NCM-300 cycles 0.83 (5.44) 0.80 (44.58) 0.15 (8.29) 0.05 (2.48)