Skip to main content
. Author manuscript; available in PMC: 2022 Mar 1.
Published in final edited form as: J Biomed Mater Res B Appl Biomater. 2020 Aug 21;109(3):338–347. doi: 10.1002/jbm.b.34703

FIGURE 6.

FIGURE 6

Loss and storage modulus (Pa) measured against an oscillation frequency (ω) range of 0 to 100 rad/s for autoclaved and nonautoclaved polymer weight fractions of (a) 30%, (b) 35%, and (c) 40%. (d) The recorded storage modulus (Pa) at 100 rad/s of autoclaved and nonautoclaved hydrogels with polymer weight fractions of 30%, 35%, and 40%. “a” denotes a significantly higher maximum recorded storage modulus than the 30% counterpart. “b” denotes a significantly higher maximum recorded storage modulus than the 35% counterpart. n = 3 for all groups. p < .05 for all differences indicated