Skip to main content
. 2021 Jun 7;11(6):1506. doi: 10.3390/nano11061506

Figure 11.

Figure 11

Abrasion morphology of the CSC coating at different CeO2 ((a) 0.01 g, (b) 0.03 g, (c) 0.05 g) and PTFE ((d) 0.1 g, (e) 0.5 g, (f) 0.7 g) contents.