Experimental design to swell and impregnate PLA with ketoprofen using scCO2.

Fixed Parameters Varying Parameters Response
Swelling study CO2 flow until target pressure
Contact time
Depressurization rate
Amount of PLA
10 g/min
0.5 h
100 bar/min
0.3 g
Pressure
Temperature
100, 250, 400 bar
35, 55, 75 °C
Swelling
SSI CO2 flow until target pressure
Contact time
Depressurization rate
Amount of PLA
Amount of KET
10 g/min
2 h
100 bar/min
0.3 g
Saturation
Pressure
Temperature
100, 250, 400 bar
35, 55, 75 °C
Swelling
Drug loading