Skip to main content
. 2021 Jun 14;12:679580. doi: 10.3389/fphar.2021.679580

FIGURE 3.

FIGURE 3

Normalized swelling ratio of CMCTS-Tk (A) and Cur@CMCTS-Tk (B) hydrogels treated with H2O2 for 0, 3, 7, and 14 days. (C) Water vapor loss of Cur@CMCTS-Tk hydrogel treated with H2O2 for 0, 3, 7, and 14 days. (D) Frequency-dependent (from 0.1 to 10 Hz), (E) strain sweeping (at a maximum strain 10%), and (F) oscillatory mode with a frequency (1.0 and 100 Hz) of storage modulus (G′).