Skip to main content
. 2021 Jun 25;13(3):144–151. doi: 10.4047/jap.2021.13.3.144

Fig. 3. Scanning electron microscope images of the worn resin surfaces after 30,000 and 60,000 cycles of chewing simulation. Crack lines are shown on the surfaces of specimens that simulated chewing for 60,000 cycles. (A) Original magnification: ×200, (B) Original magnification: ×1,000.

Fig. 3