. 2021 May 7;60(24):13621–13625. doi: 10.1002/anie.202103182

Figure 1.

Figure 1

Thickness evolution of PNIPAAm brushes on silicon substrate against the polymerization time, [NIPAAm]=2.36 M (a) and, the thickness vs. the concentration of NIPAAm, polymerization time, 30 min (b). c) Thickness characterization of 11 different polymer‐coated surfaces (polymerization time, 30 min). d) Copolymerization of two different monomers, [DMAEA]=1.65 M, [HEA]=2.18 M, PDMAEA‐b‐PHEA‐b‐PDMAEA‐b‐PHEA via PSI‐CuCRP.