Skip to main content
. 2021 Jun 29;76:105655. doi: 10.1016/j.ultsonch.2021.105655

Table 1.

Particle size, polydispersity index and zeta potential of untreated and US- treated resistant starch from lotus stem.

Sample Power (W) Hydrodynamic diameter Polydispersity index (PI) Zetapotential (mV)
RS 12.8 ± 0.09 µm 0.543 ± 0.34 −12.34 ± 0.38
URS1 100 W 765.11 ± 0.78 nm 0.413 ± 0.01 −14.09 ± 0.42
URS2 200 W 544.32 ± 1.23 nm 0.400 ± 0.05 −18.67 ± 0.01
URS3 300 W 413.19 ± 0.03 nm 0.342 ± 0.01 −20.18 ± 0.32
URS4 400 W 385.69 ± 0.15 nm 0.310 ± 0.32 −26.09 ± 0.99

Where PI = Polydispersity index; RS is the resistant starch from lotus stem; US is ultrasonication; URS1, URS2, URS3 and URS4 represent the resistant starch ultrasonicated at 100, 200, 300 and 400 W.