Skip to main content
. 2021 Jun 25;12:687118. doi: 10.3389/fmicb.2021.687118

TABLE 1.

Roughness measurements calculated by SPIPTM from the AFM topography images.

Polymer type Average roughness Sa (nm) Root mean squae roughness Sq (nm) Surface skewness Ssk (nm) Surface kurtosis Sku (nm) Peak to peak Sz (nm)
PET Unconditioned 2.6 4.9 3.9 137.8 376.0
24-h conditioning 2.9 6.9 13.4 389.7 537.2
PLA Unconditioned 9.8 15.7 −2.2 9.6 506.8
24-h conditioning 12.9 19.6 −1.7 10.3 425.1