Skip to main content
. 2021 Jun 24;14(13):3513. doi: 10.3390/ma14133513

Table 2.

Rat ectopic and bone defect models.

Rat Ectopic Model
Author (Year) Carrier BMP Dose (µg) Time (Weeks) Sample Size (n)
Kuboki et al. (1998) HA 1, 2, 3, and 4
Tsuruga et al. (1998) HA 4 1, 2, 3, and 4 3
Alam et al. (2000) TCP, HA, BCP 1.5 and 10 2 and 4 3
Vehof et al. (2002) HA 8 3, 5, 7, and 9 3
Kim Chang-Sung et al. (2004) TCP, Collagen 5 2 and 8 10
Tazaki et al. (2006) HA 0.5, 1, and 5 3
Tazaki et al. (2008) HA, TCP 0.5, 1, and 5 3 3
Luca et al. (2010) Chitosan/Hyaluronan hydrogel 150 3 3, 6
Reves et al. (2011) Chitosan-nano-HA 36 4 6
Park et al. (2011) BCP 2.5 2 and 8 5–8
Bhakta et al. (2012) Hyaluronan-based hydrogel 5 8 6
Strobel et al. (2012) BCP 1.6 2, 4, and 6 6
Kisiel et al. (2013) Hyaluronan hydrogel/Fibronectin fragments 4 7 6
Ma et al. (2014) BCP 20 8 6
Mumcuoglu et al. (2018) Collagen-based microspheres/Alginate 0.3, 1, and 10 10 8
Lin et al. (2019) Coralline HA 20 5 6
Rat Calvarial Defect Model
Author (Year) Carrier BMP Dose ( µg) Time
(Weeks)
Sample Size (n)
Jung et al. (2006) TCP 2.5 2 and 8 20
Kim et al. (2011) BCP 50 and 250 2 and 8 20
Park et al. (2011) BCP 2.5 2 and 8 5–8
Notodihardjo et al. (2011) HA 10 4 5
Jang et al. (2012) BCP 2.5, 5, 10, and 20 2 and 8 8
Lee JH et al. (2013) TCP, HA, BCP 5 4 and 8 13
Bae et al. (2017) PCL/TCP 5 4 7
Rat Femoral Defect Model
Author (Year) Carrier BMP Dose ( µg) Time (Weeks) Sample Size (n)
Chu et al. (2006) Poly(propylene fumarate)/TCP/DCP 10 6 and 15 4, 7
Johnson et al. (2011) Collagen,
Collagen/Heparin,
Heparin
3 12 7, 9
Diab et al. (2011) PCL/Silk fibroin hydrogel 5 12 10
Lee et al. (2012) BCP 1000 4 and 8 6
Rodriguez-Evora et al. (2013) Segmented polyurethane/PLGA/ TCP ceramics 1.6 and 6.5 12 9
Wai-Ching et al. (2014) Bioactive glass/DCP 10 15 8, 9
Williams et al. (2015) Collagen 25, 50, 75 and 100 8 8, 11
Krishnan et al. (2015) Nanofiber mesh alginate 5 µg 12 14