. 2021 Jun 29;14(13):3620. doi: 10.3390/ma14133620

Table 6.

Changes in linear dimensions (∆l), volume (∆V), and mass (∆m) after conditioning at –20 and +70 °C, of PUR composites.

Sample Temperature of −20 °C Temperature of +70 °C
∆l (%) ∆V (%) ∆m (%) ∆l (%) ∆V (%) ∆m (%)
PUR_REF 1.79 ± 0.01 1.66 ± 0.01 1.77 ± 0.01 1.74 ± 0.01 1.43 ± 0.01 1.52 ± 0.01
PUR_AS_C_1 1.76 ± 0.01 1.64 ± 0.01 1.69 ± 0.01 1.68 ± 0.01 1.42 ± 0.01 1.49 ± 0.01
PUR_AS_C_2 1.78 ± 0.01 1.71 ± 0.01 1.78 ± 0.01 1.63 ± 0.01 1.40 ± 0.01 1.55 ± 0.01
PUR_AS_C_5 1.84 ± 0.01 1.79 ± 0.01 1.81 ± 0.01 1.79 ± 0.01 1.50 ± 0.01 1.61 ± 0.01