Skip to main content
. 2021 Jun 28;14(13):3616. doi: 10.3390/ma14133616

Table 2.

Failure modes of specimens with 0° cracks.

Specimen Failure Mode Note
S1-1 Not conducted Unaccepted mode
S2-1 Not conducted Unaccepted mode
S3-1 End crushing Unaccepted mode
S4-1 End crushing Unaccepted mode
S5-1 End crushing Unaccepted mode
S6-1 Critical failure mode Accepted mode
S7-1 Failure in the test area Accepted mode
S8-1 Failure in the test area Accepted mode
S9-1 Failure in the test area Accepted mode