Figure 6.

Figure 6

Failure locus after pull-off tests on solid oak wood: (A) adhesive failure mode on the untreated PLA/epoxy adhesive interface, (B) adhesive failure mode on the treated PLA/wood interface, and (C) mixed adhesive/cohesive failure mode on the treated PLA/wood interface.