Skip to main content
. 2021 Jan 22;54(3):1203–1215. doi: 10.1021/acs.macromol.0c02543

Figure 1.

Figure 1

Diagram of the SVA setup for UHMW films. Films of PS-b-P2VP are spin-coated onto Si substrates and then solvent vapor annealed inside the chamber while the film thickness is monitored in situ using a reflectometer.