Polyesters Mn Theoreticalb (g mol−1) Mn Experimentalc (g mol−1) PDI
G2-HP 1179 1700 ± 180 1.32 ± 0.02
G2-HP-DTT 2986 2530 ± 580 1.39 ± 0.13
G3-HP 2573 2820 ± 270 1.44 ± 0.13
G3-HP-DTT 4950 4430 ± 260 1.28 ± 0.12
G4-HP 5359 3570 ± 420 1.56 ± 0.11
G4-HP-DTT 9525 6240 ± 980 1.12 ± 0.00
a

n ≥ 3 separate syntheses.

b

Theoretical molar mass of thiol-modified HP derived from the experimental molar mass of HP and corresponding amount of dithiols modification for each polyesters.