Table 2.
Sample | Stage |
Tonset (°C) |
Tmax (°C) |
Tendset (°C) |
Wm (%) |
Wrez (%) |
---|---|---|---|---|---|---|
CG | I | 38 | 79 | 112 | 19.96 | |
II | 237 | 301 | 330 | 56.56 | ||
III | 377 | 434 | 479 | 14.17 | 18.3 | |
CG.F10 | I | 42 | 64 | 101 | 6.53 | |
II | 171 | 203 | 235 | 24.75 | ||
III | 262 | 296 | 345 | 24.75 | ||
IV | 345 | 440 | 481 | 13.54 | 28.9 |
Tonset—onset temperature of thermal degradation; Tmax—temperature that corresponds to the maximum rate of thermal decomposition for each stage evaluated from the peaks of the DTG curves; Tendset—endset temperature of thermal degradation; Wm—mass loss rate corresponding to each thermal degradation stage; Wrez—percentage of residue remained at the end of thermal degradation (700 °C).