Table 6. Cs Concentration in the HCIL and the Salt after Salt Treatment Using the Porous MgO Crucible at 700 °C.

content amount
Cs concentration in the HCIL before the salt treatment 2430 ppm
HCIL loading weight 3.11 g
Cs weight in the HCIL 7557.3 μg
salt loading weight 77.92 g
Cs concentration in the salt after treatment 99.5 ppm
Cs weight gain in the salt 7753.0 μg